Anticorrosive environment-friendly spray paint formula

A paint and environmental protection technology, applied in anti-corrosion coatings, epoxy resin coatings, coatings, etc., can solve problems such as spraying workers' health hazards, affecting users' health, environmental pollution, etc., and achieves good environmental protection effects, good light resistance, and gloss high degree of effect

Inactive Publication Date: 2015-12-30
王海平
View PDF2 Cites 18 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

It cannot be used in occasions that require high light resistance. Among the existing oil-based paints, many paints use solvents such as benzene, ketones, and esters in the production process. These solvents are extremely volatile. During production and use It will cause pollution to the environment, and will also cause varying degrees of harm to the health of sprayi...

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Anticorrosive environment-friendly spray paint formula
  • Anticorrosive environment-friendly spray paint formula

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0019] An anti-corrosion and environment-friendly spray paint formula, the composition ratio (parts by mass) of the anti-corrosion and environment-friendly spray paint formula includes 28 parts of glacial acetic acid, 3 parts of organic fluorine epoxy resin, 7 parts of epoxy modified silicone resin solution Parts, 2 parts of ethylene glycol monomethyl ether, 6 parts of dimethyl sulfoxide, 8 parts of zinc phosphate, 8 parts of barium chromate, 1 part of ethanol, 2 parts of polyacrylate, 1 part of alcohol-soluble resin, 7 parts of diacetone alcohol , 6 parts of zinc oxide, 8 parts of toluene diisocyanate, 3 parts of butyl acetate, 12 parts of benzophenone, 9 parts of triethanolamine and 3 parts of diphenylpolysiloxane.

[0020] The preparation process of the anti-corrosion and environmentally friendly spray paint is carried out according to the following steps: Preparation of mixture A: take a heatable container, pour glacial acetic acid and epoxy-modified silicone resin liquid i...

Embodiment 2

[0021] Example 2: The rest are the same as in Example 1, except that 29 parts of glacial acetic acid, 4 parts of organic fluorine epoxy resin, 8 parts of epoxy-modified silicone resin liquid, 2 parts of ethylene glycol monomethyl ether, and 7 parts of dimethyl sulfoxide 9 parts of zinc phosphate, 9 parts of barium chromate, 2 parts of ethanol, 3 parts of polyacrylate, 2 parts of alcohol-soluble resin, 8 parts of diacetone alcohol, 7 parts of zinc oxide, 9 parts of toluene diisocyanate, 4 parts of butyl acetate parts, 13 parts of benzophenone, 10 parts of triethanolamine and 4 parts of diphenyl polysiloxane; in the step (1), the heating temperature is 85°C; in the step (5), at 40°C Add water for dilution, the amount of added water is 8 parts, and then continue to stir for a period of time, and the duration of stirring is 37 minutes.

Embodiment 3

[0022] Example 3: The rest are the same as in Example 1, except that 30 parts of glacial acetic acid, 5 parts of organic fluorine epoxy resin, 9 parts of epoxy-modified silicone resin liquid, 3 parts of ethylene glycol monomethyl ether, dimethyl methylene 8 parts of sulfone, 10 parts of zinc phosphate, 10 parts of barium chromate, 3 parts of ethanol, 4 parts of polyacrylate, 3 parts of alcohol-soluble resin, 9 parts of diacetone alcohol, 8 parts of zinc oxide, 10 parts of toluene diisocyanate, butyl acetate 5 parts of ester, 14 parts of benzophenone, 11 parts of triethanolamine and 5 parts of diphenylpolysiloxane; in the step (1), the heating temperature is 90°C; Add water at ℃ for dilution, the amount of water added is 9 parts, and then continue to stir for a period of time, and the duration of stirring is 39 minutes.

[0023] After the above process steps, the paint sample is taken out to be tested:

[0024]

[0025] From the above data, it can be known that the shelf ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses an anticorrosive environment-friendly spray paint formula, and relates to the field of chemical industries. The anticorrosive environment-friendly spray paint formula comprises the following components in parts by weight: 28 to 35 parts of glacial acetic acid, 3 to 7 parts of organic fluorine epoxy resin, 7 to 12 parts of epoxy modified organic silicon resin, 2 to 6 parts of glycol monomethyl ether, 6 to 9 parts of dimethyl sulfoxide, 8 to 13 parts of zinc phosphate, 8 to 13 parts of barium chromate, 1 to 4 parts of ethanol, 2 to 7 parts of polyacrylate, 1 to 4 parts of alcohol soluble resin, 7 to 13 parts of diacetone alcohol, 6 to 9 parts of zinc oxide, 8 to 13 parts of toluene diisocynate, 3 to 7 parts of n-butyl acetate, 12 to 16 parts of benzophenone, 9 to 13 parts of triethanolamine and 3 to 7 parts of diphenyl polysiloxane. The paint is bright in color and good in air-curing resisting effect, can substitute medium chrome yellow in inorganic pigment, is applicable to the outer wall paint, and has no harm of heavy metals, no harmful substances, good environment protection effect, little odor, no peculiar smell after being smeared on the wall, good mechanical performance, excellent electric insulation performance, dampness and water resistance, rust and cold resistance and ozone aging resistance.

Description

technical field [0001] The invention relates to the field of chemical industry, in particular to an anti-corrosion and environment-friendly spray paint formula. Background technique [0002] Outdoor long-term protective coatings generally require coating protection life of more than 10a, which belongs to the long-term protective coating system, which can be applied in harsh application environments and has a long service life. At present, large-scale mechanical equipment that has been used for a long time or large-scale mechanical equipment that operates in the open air is severely corroded after being exposed to wind and rain, which is likely to cause unsafe hazards and shorten the service life. The comprehensive properties of traditional paints such as light fastness, heat resistance, and migration resistance are relatively poor. It is mainly used for general quality air-dry paint, latex paint, printing ink, paint and other low-level applications. It cannot be used in oc...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C09D175/04C09D183/04C09D163/00C09D133/04C09D5/08C09D7/12
Inventor 王海平
Owner 王海平
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products