A kind of preparation method of hardened coating of weaving paper
A hard coating and boiling technology, applied in the field of woven art, can solve the problems affecting the artistry and practicability of paper woven products, restrict the development of paper woven materials, and deform the soft couch, and achieve the goal of maintaining artistry, good waterproof, and enhanced adhesion. The effect of knot
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A hardened coating for weaving paper, made of the following raw materials in parts by weight: 8 parts of polyurethane, 6 parts of petroleum resin, 7 parts of hydroxypropyl methylcellulose, 10 parts of polyacrylate latex, glutinous rice 6 parts, 5 parts of cotton seed husk, 3 parts of lithium carbonate, 3 parts of boron nitride fiber, 3 parts of tert-butyl peroxybenzoate, 4 parts of fluorocarbon emulsion, 4 parts of ammonium persulfate, 2 parts of acrylic acid, 39 parts of water .
[0013] A preparation method for a hardened coating of paper for weaving, comprising the following steps:
[0014] (1) Put the cotton seed husk in boiling water equivalent to 5 times its weight and cook for 1.5-2 hours, then continue to add glutinous rice and cook for 35-45 minutes, stir once every 15 minutes during the cooking process, boil After the cooking is completed, filter out the soup juice, mash the filtered mixture for 5-8 minutes, then add 20% by weight of sodium hydroxide solution...
Embodiment 2
[0018] A hardened coating of paper for weaving, made of the following raw materials in parts by weight: 6 parts of polyurethane, 8 parts of petroleum resin, 6 parts of hydroxypropyl methylcellulose, 12 parts of polyacrylate latex, glutinous rice 8 parts, 3 parts of cotton seed husk, 1 part of lithium carbonate, 2 parts of boron nitride fiber, 3 parts of tert-butyl peroxybenzoate, 2 parts of fluorocarbon emulsion, 6 parts of ammonium persulfate, 1 part of acrylic acid, 42 parts of water .
[0019] Its preparation method is the same as in Example 1.
Embodiment 3
[0021] A hardened coating for weaving paper, made of the following raw materials in parts by weight: 10 parts of polyurethane, 5 parts of petroleum resin, 4 parts of hydroxypropyl methylcellulose, 10 parts of polyacrylate latex, glutinous rice 5 parts, 6 parts of cotton seed hulls, 1 part of lithium carbonate, 3 parts of boron nitride fiber, 4 parts of tert-butyl peroxybenzoate, 2 parts of fluorocarbon emulsion, 3 parts of ammonium persulfate, 2 parts of acrylic acid, 45 parts of water .
[0022] Its preparation method is the same as in Example 1.
[0023] After the hardened coating prepared in the examples is used on the surface of the weaving paper, the thickness is 0.02-0.04mm, which increases the hardness and wear resistance of the weaving paper. Under the condition of -10-40°C, the hardness changes little, It has good water resistance and can be used for more than 15 years without deformation, which improves the durability and weather resistance of paper woven products.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information