Sulfur-supported feedstuff addictive and preparation method thereof
A feed additive and elemental sulfur technology, which is applied in the field of hydrotalcite loaded elemental sulfur and its preparation, can solve the problems of cross-infection of pathogenic bacteria, economic losses of farmers, disease outbreaks, etc., and achieve inhibition of proliferation, good biocompatibility and gastrointestinal The effect of tract mucosa affinity, uniform dispersion and stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Preparation: According to "Oral vanadium supplementation agent with double metal oxide as carrier and its preparation and application method" (see: Ye Ying, Feng Lujia, Zheng Libo, Shen Zhongyue, Han Jie, Chen Zhifei, Li Shanshan. National Invention Patent Authorization Announcement No. CN 1187091C) method to prepare hydrotalcite.
[0024] 1) Grind the hydrotalcite obtained in the preparatory step to 400 mesh, add water and stir evenly, and make a suspension slurry with a concentration of 10%:
[0025] 2) Slowly add sodium sulfite with a sulfur content of 1% by hydrotalcite weight and sodium sulfide with a molar ratio twice that of sodium sulfite to the suspension in step 1) under stirring, and then add dilute sulfuric acid with a molar concentration of 0.5moL / L , adjust pH=3.0, react at room temperature for 5 hours;
[0026] 3) centrifugal dehydration of the suspension slurry in step 2);
[0027] 4) drying and pulverizing the filter cake obtained in step 3) to 300 me...
Embodiment 2
[0029] Preparation: According to "A Method for Preparing Bimetallic Oxide and Hydrotalcite" (see: Ye Ying, Li Shanshan, Chen Zhifei, Zheng Libo, Huang Xia, Wu Daidai, Han Jie, Zhang Weirui. National Invention Patent Grant No. CN 1222467C) method Preparation of hydrotalcite.
[0030] 1) Grind the hydrotalcite obtained in the preparatory step to 500 mesh, add water and stir evenly, and make a suspension slurry with a concentration of 5%:
[0031] 2) Slowly add sodium bisulfite with a sulfur content of 5% by weight of hydrotalcite and sodium sulfide with a molar ratio twice that of sodium bisulfite to the suspension slurry in step 1) under stirring, and then add a molar concentration of 1.5 MoL / L dilute sulfuric acid, adjust pH=5.0, react at room temperature for 8 hours;
[0032] 3) the suspension slurry in step 2) is filtered and dehydrated;
[0033] 4) drying and crushing the filter cake obtained in step 3) to 400 meshes to obtain a loaded elemental sulfur feed additive. The...
Embodiment 3
[0035] 1) Grind commercially available hydrotalcite to 500 mesh, add water and stir evenly to make a suspension slurry with a concentration of 1%:
[0036] 2) Sodium sulfite heptahydrate (Na 2 SO 3 ·7H 2 (2) and sodium sulfide whose molar ratio is 2 times that of sodium sulfite are slowly added to the suspension slurry of step 1) under stirring, and then dilute sulfuric acid with a molar concentration of 1.5moL / L is added to adjust pH=4.0, and react at room temperature for 10 hours;
[0037] 3) the suspension slurry in step 2) is filtered and dehydrated;
[0038]4) drying and crushing the filter cake obtained in step 3) to 400 meshes to obtain a loaded elemental sulfur feed additive. The content of sulfur in hydrotalcite is 10%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com