Nano-biological water body remediation agent for aquaculture and preparation method thereof
A technology for water body restoration and aquaculture, applied in biological water/sewage treatment, chemical instruments and methods, water/sludge/sewage treatment, etc., can solve the problems of difficult indigenous microorganisms, low community stability, and natural bioremediation efficiency and slow speed
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 3
[0062] In Example 3, Rhodopseudomonas palustris ACCC 00309 and Pseudomonas putida ACCC 01017 used were purchased from China Agricultural Microorganism Culture Collection Center (ACCC); Vibrio Fischer CICC 10483 and Bacillus subtilis CICC 20682 purchased from China Industrial Microorganism Culture Collection Center (CICC).
Embodiment 1
[0063] The preparation of embodiment 1 aquaculture nanobiological water restoration agent
[0064] (1) Preparation of nano tourmaline
[0065] Pour the natural magnesium tourmaline mineral into a jaw crusher and crush it to prepare tourmaline particles with a particle size of 20,000 mesh. The processing equipment used is general-purpose equipment.
[0066] (2) Preparation of Nano Titanium Dioxide
[0067] Titanium sulfate is used as raw material, urea is used as precipitating agent, it is added into the reactor, and pressurized at 120°C for 2 hours. The precipitate is dried in a vacuum drying oven, the temperature is controlled at 50-70°C, and the vacuum degree is 96kPa. The dried precipitate is put into a resistance furnace and calcined to obtain nano-titanium dioxide with an average particle size of 30nm, which is ready for use.
[0068] (3) Zeolite modification
[0069] Pour the natural zeolite block into a jaw crusher for crushing, then further grind it with a disc mill...
Embodiment 2
[0078] The preparation of embodiment 2 aquaculture nanobiological water restoration agent
[0079] (1) Preparation of nano tourmaline
[0080] Pour the natural magnesium tourmaline mineral into a jaw crusher and crush it to prepare tourmaline particles with a particle size of 14,000 mesh. The processing equipment used is general-purpose equipment.
[0081] (2) Preparation of Nano Titanium Dioxide
[0082] Titanium sulfate is used as raw material, urea is used as precipitating agent, it is added into the reactor, and pressurized at 120°C for 2 hours. The precipitate is dried in a vacuum drying oven, the temperature is controlled at 50-70°C, and the vacuum degree is 96kPa. The dried precipitate is put into a resistance furnace and calcined to obtain nano-titanium dioxide with an average particle size of 80nm, which is ready for use.
[0083] (3) Zeolite modification
[0084] Pour the natural zeolite block into a jaw crusher for crushing, then further grind it with a disc mill...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com