Preparation method of defoamer for textile printing and dyeing
A textile printing and dyeing, defoaming agent technology, applied in the field of defoaming agents, can solve the problems of poor dispersion of silicone, no defoaming activity, too large particle size, etc., and achieve good defoaming, improved viscosity, and stable quality.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A kind of defoamer for textile printing and dyeing, in parts by mass, is made by following steps:
[0021] S1, after mixing 20 parts of polydimethylsiloxane, 8 parts of high carbon alcohol, 4 parts of zinc stearate, 5 parts of tributyl phosphate, 4 parts of monoglyceride fatty acid ester, and 0.5 part of potassium hydrogen persulfate, Stir evenly to prepare liquid A;
[0022] S2, add 3 parts of sodium hexametaphosphate, 2 parts of sorbitan fatty acid and 3 parts of carboxymethyl cellulose into 85 parts of deionized water, and stir evenly to obtain liquid B;
[0023] S3, mix liquid A and liquid B at 70°C, heat up to 100°C and stir evenly, then add 15 parts of hydrophobic silicon dioxide and keep warm for 30 minutes to prepare a defoamer for textile printing and dyeing.
Embodiment 2
[0025] A kind of defoamer for textile printing and dyeing, in parts by mass, is made by following steps:
[0026] S1, after mixing 30 parts of polymethyltriethoxysilane, 5 parts of higher carbon alcohol, 5 parts of zinc stearate, 8 parts of tributyl phosphate, 2 parts of monoglyceride fatty acid ester, and 2 parts of potassium hydrogen persulfate , and stir evenly to prepare liquid A;
[0027] S2, add 3 parts of sodium hexametaphosphate, 5 parts of polysorbate and 1.5 parts of carboxyethyl cellulose into 70 parts of deionized water, and stir evenly to prepare liquid B;
[0028] S3, mix liquid A and liquid B at 60°C, heat up to 90°C and stir evenly, then add 30 parts of hydrophobic silicon dioxide and 3 parts of antifoaming agent for textile printing and dyeing, and keep warm for 40 minutes to prepare the antifoaming agent for textile printing and dyeing foaming agent.
Embodiment 3
[0030] A kind of defoamer for textile printing and dyeing, in parts by mass, is made by following steps:
[0031] S1, after mixing 40 parts of polymethyltrimethoxysilane, 15 parts of higher carbon alcohol, 5 parts of zinc stearate, 6 parts of tributyl phosphate, 4 parts of monoglyceride fatty acid ester, and 1 part of potassium hydrogen persulfate, Stir evenly to prepare liquid A;
[0032] S2, add 2 parts of sodium hexametaphosphate, 3 parts of fatty acid esters of glycerol and 2 parts of xanthan gum into 75 parts of deionized water, and stir evenly to prepare liquid B;
[0033] S3, mix liquid A and liquid B at 65°C, heat up to 95°C and stir evenly, then add 20 parts of hydrophobic silicon dioxide, 2 parts of defoamer for textile printing and dyeing, and 2 parts of glutaraldehyde, and keep warm for 35 minutes. Prepare the defoamer for textile printing and dyeing.
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com