A rare earth modification, water processor technology, applied in water/sewage treatment, chemical instruments and methods, water/sludge/sewage treatment, etc., can solve the problems of short-lived active elements, threatening biological life, and adverse human health. , to achieve the effect of increasing the content of biological enzymes, promoting metabolism, and obvious health care effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] The proportion of each component of the material is as follows: gray iron (the content of carbon, manganese, phosphorus, sulfur and silicon is normal, in line with the relevant national standards. The same below) 100kg, mixed rare earth 3kg, metal zinc 3kg, titanium oxide powder 0.6kg.
[0016] Use an electric furnace for melting.
[0017] Pour the pig iron weighed according to the proportion into the electric furnace, melt it into molten iron, then add the mixed rare earth, metal zinc, and titanium oxide powder into the molten iron, and fully stir evenly. At this time, the temperature of the molten iron exceeds 1450°C. After 1350°C, it is poured into the inner tank mold or end cap mold of the water processor, and after cooling, the rare earth modified iron alloy inner tank blank or end cover blank of the health care water treatment device is obtained.
[0018] Water is treated through the health care water processor (abbreviation "BCC health care water processor") that...
Embodiment 2
[0049] The proportion of each component of the material is as follows: gray iron 100kg, rare earth 4kg, metal zinc 4kg, titanium oxide powder 0.8kg, zinc oxide 0.5g.
[0050] Melted in a cupola furnace. Melting, casting method are with embodiment 1.
Embodiment 3
[0052] The proportion of each component of the material is as follows: gray iron 100kg, rare earth 2.5kg, metal zinc 2.5kg, titanium oxide powder 0.5kg, platinum 0.7kg, vanadium 0.3kg.
[0053] Using electric furnace melting. Melting, casting method are with embodiment 1.
[0054] The rare earth modified iron alloy of this embodiment is particularly suitable for casting inner tanks or / and end caps of water processors for treating arsenic-containing water.