A nanotechnology of madecassic acid and solid lipids, which is applied in the field of medicine, can solve the problems of low skin penetration and drug utilization, large molecular weight, and low water solubility, and achieve improved keratinization function and good biocompatibility , the effect of avoiding liver damage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0044] Preferably, the preparation method of the Asiatic Hydroxy Acid Solid Lipid Nanoparticle Gel comprises:
[0045] (1) After mixing glyceryl behenate and soybean phospholipid, heat and melt in a water bath at 85-95°C;
[0046] (2) After adding madecassic acid to absolute ethanol and ultrasonically dissolving it, adding it to the molten liquid of step (1), heating and melting in a water bath at 85-95°C to form an oil phase;
[0047] (3) Disperse the surfactant in water, heat and melt in a water bath at 85-95°C to form a water phase;
[0048] (4) Slowly add the oil phase to the water phase under stirring at a constant temperature of magnetic force of 1000r / min and stir for 40min. After mixing evenly, shear at 13000r / min for 2-5min to form colostrum;
[0049] (5) Prepare the colostrum into Asiatic acid solid lipid nanoparticles by solvent emulsification volatilization-high pressure homogenization method;
[0050] (6) Take carbomer 940 and water in a weight ratio of 1:7.5-12.5 and mix an...
Embodiment 1
[0057] (1) After mixing 300 g of glyceryl behenate and 150 g of soybean phospholipid, heat and melt in a water bath at 85°C;
[0058] (2) After adding 150 g of madecassic acid to 6 g of absolute ethanol to ultrasonically dissolve it, adding it to the molten liquid of step (1), heating and melting in a water bath at 85° C. to form an oil phase;
[0059] (3) Disperse 750g of surfactant (the ratio of Tween-80 and Poloxamer 188 is 1:0.5) in water, heat and melt in a water bath at 85°C and mix uniformly to form an aqueous phase;
[0060] (4) Slowly add the oil phase to the water phase under stirring at a constant temperature of magnetic force of 1000r / min and stir for 40min, mix well and shear at 13000r / min for 2min to form colostrum;
[0061] (5) Prepare the colostrum into Asiatic acid solid lipid nanoparticles by solvent emulsification volatilization-high pressure homogenization method;
[0062] (6) Take carbomer 940 and water in a weight ratio of 1:7.5 and mix and swell for 24h. Add 0.8ml...
Embodiment 2
[0066] (1) After mixing 300 g of glyceryl behenate and 150 g of soybean phospholipids, heat and melt in a water bath at 90°C;
[0067] (2) After adding 220 g of madeasiatic acid to 8.8 g of absolute ethanol to dissolve it ultrasonically, add it to the molten liquid of step (1), and heat and melt in a water bath at 90° C. to form an oil phase;
[0068] (3) Disperse 1000 g of surfactant (the ratio of Tween-80 and Poloxamer 188 is 1:1) in water, heat and melt in a water bath at 90°C and mix uniformly to form an aqueous phase;
[0069] (4) Slowly add the oil phase to the water phase under stirring at a constant temperature of magnetic force of 1000r / min and stir for 40min, mix well and shear at 13000r / min for 3min to form colostrum;
[0070] (5) Prepare the colostrum into Asiatic acid solid lipid nanoparticles by solvent emulsification volatilization-high pressure homogenization method;
[0071] (6) Take carbomer 940 and water in a weight ratio of 1:10 and mix for 24h, add 0.8ml of ethanol ...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
electric potential / voltage | aaaaa | aaaaa |
polydispersity index | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com