A high-performance near-pure
zinc alloy and its preparation method and application, belonging to the technical field of
zinc alloys. The
alloy composition is that the Zn content is ≥99.5%, and the remaining trace
alloy elements include at least 2 of the following 14 elements: Mg, Mn, Li, Cu, Ag, Ca, Sr, Fe, Zr, Ti, Al, C, Ga, Si. The yield strength of the alloy is ≥250MPa, the tensile strength is ≥320MPa, the elongation is ≥25%, the
mechanical property change in
room temperature storage within 1 year is ≤5%, the maximum
bending force is ≥2kN, the stress
corrosion sensitivity factor is ≤15%, the
corrosion pit size is ≤15μm after immersion for 60 days, and the standard deviation of the
corrosion pit size is ≤3μm. The alloy is suitable for the preparation of degradable stents,
bone implant devices, intestinal, vascular or neural
anastomosis devices or staples, vascular clips, guided bone and tissue regeneration membranes,
artificial heart valves, meningeal repair membranes, soluble bridge plugs for oil drills, fracturing balls,
zinc alloy die castings, electrogalvanized materials, construction zinc materials, zinc materials for batteries, zinc materials for printing, and zinc-based alloy solders.