Embodiment 1
[0025] This embodiment relates to a desiccant, including the following raw materials in parts by weight: 20 parts of bentonite, 20 parts of attapulgite clay, 10 parts of montmorillonite, 8 parts of plant starch, 5 parts of superabsorbent resin, 15 parts of calcium chloride, 1 part of scrap iron, 6 parts of modified turbidite, and 2 parts of fungicide.
[0026] Wherein, the modified zeolite is prepared by the following method: put the zeolite into the mixed solution of sodium carbonate and potassium permanganate and soak it for 3 hours, take it out and dry it, and add a silane coupling agent equivalent to 3% by weight of the zeolite KH550, sodium lauryl sulfate equivalent to 2% of the weight of the zeolite and alumina equivalent to 2% of the weight of the zeolite were stirred at 1000r / min for 10 minutes, then ground, and passed through a 120-160 mesh sieve to obtain the modified zeolite.
[0027] Wherein, the vegetable starch is corn starch.
[0028] Wherein, the bactericide i...
Embodiment 2
[0036] This embodiment relates to a desiccant, including the following raw materials in parts by weight: 40 parts of bentonite, 40 parts of attapulgite clay, 20 parts of montmorillonite, 17 parts of plant starch, 10 parts of superabsorbent resin, 25 parts of calcium chloride, 2 parts of scrap iron, 13 parts of modified zeolite, 3 parts of fungicide.
[0037] Wherein, the modified zeolite is obtained by the following method: put the zeolite into the mixed solution of sodium carbonate and potassium permanganate and soak it for 3 hours, take it out and dry it, and add a silane coupling agent equivalent to 3% by weight of the zeolite KH550, sodium lauryl sulfate equivalent to 2% of the weight of the zeolite and alumina equivalent to 2% of the weight of the zeolite were stirred at 1000r / min for 10 minutes, then ground, and passed through a 120-160 mesh sieve to obtain the modified zeolite.
[0038] Wherein, the vegetable starch is wheat starch.
[0039] Wherein, the bactericide is...
Embodiment 3
[0047] This embodiment relates to a desiccant, including the following raw materials in parts by weight: 25 parts of bentonite, 26 parts of attapulgite clay, 14 parts of montmorillonite, 10 parts of plant starch, 6 parts of superabsorbent resin, 18 parts of calcium chloride, 1.3 parts of scrap iron, 7 parts of modified turbidite, and 2.4 parts of fungicide.
[0048]Wherein, the modified zeolite is prepared by the following method: put the zeolite into the mixed solution of sodium carbonate and potassium permanganate and soak it for 3 hours, take it out and dry it, and add a silane coupling agent equivalent to 3% by weight of the zeolite KH550, sodium lauryl sulfate equivalent to 2% of the weight of the zeolite and alumina equivalent to 2% of the weight of the zeolite were stirred at 1000r / min for 10 minutes, then ground, and passed through a 120-160 mesh sieve to obtain the modified zeolite.
[0049] Wherein, the vegetable starch is corn starch.
[0050] Wherein, the bacteric...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com