Water-based paint which has high thermal dissipation and is applied to wooden door

A water-based, high heat dissipation technology, applied in the direction of fireproof coatings, epoxy resin coatings, coatings, etc., can solve the problems of volatile toxic gases, poor flame retardancy, poor heat dissipation effect, etc., and achieve good compactness and flame retardancy Good, excellent adhesion effect

Inactive Publication Date: 2018-05-11
合肥林邦门业有限公司
View PDF1 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] Although there are many types of existing wooden door coatings, they generally have the disadvantages of poor flame retardancy, volatile toxic gases, and poor heat dissipation effects, which cannot meet the various needs of people.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0019] A water-based coating for high heat dissipation wooden doors, its raw materials include: 50kg of main ingredients, 2kg of C9 petroleum resin, 0.1kg of catalyst, 2kg of water-soluble melamine-formaldehyde resin, 0.2kg of cocamidopropyl betaine, and octylphenol polyoxyethylene ether 0.6kg, composite flame retardant 1kg, illite 8kg, quartz sand 3kg, diatomite 4kg, heavy calcium carbonate 1kg, coal gangue powder 8kg, hollow glass beads 1kg, anti-sedimentation agent 3kg, dispersant 1kg, flow Leveling agent 2kg, defoamer 1kg.

[0020] The main ingredients include: 50kg of water-based bisphenol A epoxy resin, 5kg of epoxy modified alkyd resin.

[0021] The composite flame retardant is prepared by the following process: mix 80kg of stearic acid, 2kg of xylitol, and 2kg of dimethylcyclosiloxane, stir for 15 minutes under nitrogen protection, and dehydrate at a stirring temperature of 130°C, add 10kg of expanded graphite, 4kg of Grind sodium chloride for 5 minutes, add 100kg of ...

Embodiment 2

[0023] A water-based coating for high heat dissipation wooden doors, its raw materials include: 70kg of main ingredients, 1kg of C9 petroleum resin, 0.2kg of catalyst, 1kg of phenol-blocked isocyanate-based polyurethane resin, 0.8kg of cocamidopropyl betaine, octylphenol polyoxygen Vinyl ether 0.4kg, composite flame retardant 4kg, illite 2kg, quartz sand 5kg, diatomaceous earth 1kg, heavy calcium carbonate 2kg, coal gangue powder 2kg, hollow glass beads 4kg, anti-sedimentation agent 1kg, dispersant 3kg , leveling agent 0.5kg, defoamer 2kg.

[0024] The main ingredients include: 40kg of water-based bisphenol A epoxy resin, 15kg of epoxy modified alkyd resin.

[0025] The composite flame retardant is prepared by the following process: mix 60kg of stearic acid, 6kg of xylitol, and 1kg of dimethylcyclosiloxane, stir for 25min under nitrogen protection, and dehydrate at a stirring temperature of 120°C, add 16kg of expanded graphite, 2kg of Grind sodium chloride for 12 minutes, add...

Embodiment 3

[0027] A water-based coating for high heat dissipation wooden doors, its raw materials include: 55kg of main ingredients, 1.8kg of C9 petroleum resin, 0.12kg of catalyst, 0.9kg of water-soluble melamine formaldehyde resin, 0.9kg of water-soluble phenolic resin, and 0.4kg of cocamidopropyl betaine kg, octylphenol polyoxyethylene ether 0.55kg, composite flame retardant 2kg, illite 6kg, quartz sand 3.5kg, diatomite 3kg, heavy calcium carbonate 1.3kg, coal gangue powder 6kg, hollow glass beads 2kg , Anti-settling agent 2.5kg, dispersant 1.5kg, leveling agent 1.5kg, defoamer 1.2kg.

[0028] The main ingredients include: 48kg of water-based bisphenol A epoxy resin, 8kg of epoxy modified alkyd resin.

[0029] The composite flame retardant is prepared by the following process: mix 75kg of stearic acid, 3kg of xylitol, and 1.8kg of dimethylcyclosiloxane, stir for 18 minutes under nitrogen protection, and dehydrate at a stirring temperature of 128°C, add 12kg of expanded graphite, Grin...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
Login to View More

Abstract

The invention discloses water-based paint which has high heat dissipation and is applied to a wooden door. The water-based paint is prepared from, in parts by weight, 50-70 parts of a main material, 1-2 parts of C9 petroleum resin, 0.1-0.2 part of a catalyst, 1-2 parts of a water-based curing agent, 0.2-0.8 part of cocamidopropyl betaine, 0.4-0.6 part of octylphenol polyoxyethylene ether, 1-4 parts of a composite flame retardant, 2-8 parts of illite, 3-5 parts of quartz sand, 1-4 parts of diatomaceous earth, 1-2 parts of heavy calcium carbonate, 2-8 parts of coal gangue powder, 1-4 parts of hollow glass microbeads, 1-3 parts of an anti-settling agent, 1-3 parts of a dispersant, 0.5-2 parts of a leveling agent and 1-2 parts of a defoamer. A coating of the water-based paint has strong adhesion, a full paint film, no yellowing and brittleness, no organic solvent, a good thermal dissipation effect, excellent flame-retardant performance, superior comprehensive performance and a good protection effect on the wooden door, no peeling emerges on the surface after long-term use of the wooden door, and fire can also be prevented effectively when a fire occurs.

Description

technical field [0001] The invention relates to the technical field of wooden doors, in particular to a water-based paint for wooden doors with high heat dissipation. Background technique [0002] The history of human survival and use of paint can be traced back to the Stone Age. In the last century, a variety of newly developed synthetic resin paints began to be used in a large number of pattern paints, entering an era dominated by synthetic film-forming substances. The per capita consumption of coatings in developed countries has reached more than 10kg, and the modern coatings industry has become an important industry in the modern chemical industry. [0003] Although the existing wooden door coatings are of a great variety, they generally have the disadvantages of poor flame retardancy, volatile toxic gas, and poor heat dissipation effect, which cannot meet the various needs of people. Contents of the invention [0004] Based on the technical problems in the background...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D163/00C09D5/18C09D7/61C09D7/62C09D7/65
CPCC08K2003/265C08L2205/035C09D5/18C09D163/00C08L67/08C08L57/02C08L61/28C08L71/02C08K13/06C08K9/04C08K9/06C08K9/08C08K9/02C08K7/24C08K3/16C08K7/26C08K3/26C08K7/28
Inventor 袁中领
Owner 合肥林邦门业有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products