Efficient paint fog coagulant, preparation method thereof and application
A technology of paint mist coagulant and floating agent, applied in the field of materials, can solve the problems of corrosion of circulating water equipment, increase of use cost, long operation steps, etc., and achieve the effect of saving enterprise cost, improving water quality, and simple use method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0087] Detackifier components and proportioning ratio: 50 parts of polyaluminum sulfate (the mass fraction of aluminum is 15% as aluminum oxide), 10 parts of water-soluble melamine formaldehyde resin with a viscosity of 450mpa.s (25°C rotational viscosity), sulfuric acid 30 parts of iron; 10 parts of dodecyl dimethyl benzyl ammonium bromide; mix the three through a solid powder mixer;
[0088] Preparation of slow-release floating agent: 2 parts of anionic polyacrylamide with a number average molecular weight of 12 million, 30 parts of citric acid, 20 parts of sodium carbonate / sodium bicarbonate (the mass ratio of the two is 1:20), 40 parts of mannitol , 8 parts of polyethylene glycol 4000, mixed by a mixer, made into a soft material with 5% PVP anhydrous ethanol solution, granulated with a 20-mesh nylon screen, dried at 45°C for 12 hours, and granulated with a 18-mesh.
[0089] Take 10 parts of pH regulator sodium hydroxide, 10 parts of slow-release floating agent, and 80 part...
Embodiment 2
[0092] Anti-tack agent components and ratio: 40 parts of polyaluminum iron silicate (the mass fraction of aluminum is 25% as alumina), 20 parts of cationic polyacrylamide with a number average molecular weight of 8 million, and 30 parts of aluminum chloride , 10 parts of nonylphenol polyoxyethylene ether with a molecular weight of 10,000; mix the four through a solid powder mixer;
[0093] Preparation of slow-release floating agent: 3 parts of anionic polyacrylamide with a number average molecular weight of 20 million, 35 parts of citric acid, 25 parts of sodium carbonate / sodium bicarbonate (the mass ratio of the two is 1:20), 30 parts of mannitol , Polyethylene glycol 4000 7 parts, mixed by a mixer, made soft material with 1% PVP absolute ethanol solution, granulated with 20 mesh nylon screen, dried at 45°C for 12 hours, granulated with 18 mesh
[0094] Take 15 parts of pH regulator sodium carbonate, 15 parts of slow-release floating agent, and 70 parts of anti-tack agent and...
Embodiment 3
[0097] Anti-sticking agent components and proportioning: 40 parts of polyaluminum ferric silicate (the mass fraction of aluminum is 20% as aluminum oxide), 20 parts of cationic polyacrylamide with a number average molecular weight of 1000, 30 parts of aluminum chloride, 10 parts of fatty acid methyl ester polyoxyethylene ether with a molecular weight of 20,000; the four are mixed by a solid powder mixer;
[0098] Preparation of slow-release floating agent: 3 parts of anionic polyacrylamide with a number average molecular weight of 18 million, 35 parts of citric acid, 25 parts of sodium carbonate / sodium bicarbonate (the mass ratio of the two is 1:20), 30 parts of mannitol , Polyethylene glycol 4000 7 parts, mixed by a mixer, made soft material with 1% PVP absolute ethanol solution, granulated with 20 mesh nylon screen, dried at 45°C for 12 hours, granulated with 18 mesh
[0099] Take 15 parts of potassium hydroxide as a pH adjuster, 15 parts of a slow-release floating agent, an...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com