Silica sol hybrid hydroxyl acrylate emulsion and preparing method thereof

A technology of hydroxyacrylate and silica sol, which is applied in polyurea/polyurethane coatings, coatings, paints containing biocide, etc., can solve problems such as poor gloss and fullness, easy cracking of coating films, and large volume shrinkage , to achieve the effect of improving gloss and hardness, high adhesion, and ensuring product quality

Inactive Publication Date: 2018-05-29
江苏日出化工有限公司
View PDF2 Cites 15 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] The application number is 201710102922.7, which discloses a method for preparing a core-shell structure hydroxyl acrylic emulsion, which effectively combines acrylic monomer pre-emulsification technology, seed emulsion polymerization technology, core-shell emulsion polymerization technology, self-crosslinking emulsion polymerization technology, and emulsion polymerization technology. In combination, the monomer pre-emulsification of the seed emulsion polymerization part, the direct dripping of the monomer of the core emulsion polymerization part and the pre-emulsification of the monomer of the shell emulsion polymerization part are adopted, and different initiators are selected in the core-shell emulsion polymerization process and drop rate, and the core shell is selected from anionic emulsifiers and nonionic emulsifiers with different properties to effectively control the particle size and distribution of the emulsion; in the case of no or only a small amount of gelation during the synthesis process, the emulsion The emulsifier added in the synthesis accounts for less than 6% of the total amount of acrylic monomers (accounting for less than 3% of the total amount of the synthesized emulsion), but this kind of latex mainly has low hardness, poor gloss and fullness
[0004] Silica sol is a dispersion of nano-silica in water, which contains a large number of hydroxyl groups. When silica sol loses water, monomeric silicic acid gradually polymerizes into high-polymer silica gel. With the evaporation of water, the colloidal molecules increase and finally form -SiO-O-SiO- coating film, due to Na 2 The content of O in silica sol is low. Silica sol has a certain amount of film-forming and dissolving characteristics. Its wear resistance, heat resistance, and hardness are significantly better than organic coatings. The coating film is dense and hard, and does not generate static electricity. This kind of dust is difficult to adhere to, but silica sol has the disadvantages of large volume shrinkage during film formation and easy cracking of the coating film

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Silica sol hybrid hydroxyl acrylate emulsion and preparing method thereof
  • Silica sol hybrid hydroxyl acrylate emulsion and preparing method thereof
  • Silica sol hybrid hydroxyl acrylate emulsion and preparing method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1)

[0035] (1) Add 80g of water, 1g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 20g of styrene, 100g of methyl methacrylate, and 1g of acrylic acid into the emulsification container with stirring in sequence and add it at 200r / min rotating speed to disperse at high speed to obtain pre-emulsion.

[0036] (2) Put 200g of water, 1g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 100g of butyl acrylate, 150g of cyclohexyl methacrylate, 20g of hydroxyethyl acrylate, 3g of acrylic acid, and 1g of A-171 in order Add it into an emulsification container with stirring and disperse at a high speed of 200r / min to obtain a pre-emulsion.

[0037] (3) Add 2g of nonylphenol polyoxyethylene ether, 1g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 5g of silica sol, 1g of sodium bicarbonate and 250g of water into a reaction vessel with stirring , stirring at a low speed of 50r / min and heating to 84°C, adding an aqueous solution containing 0.5g sodi...

Embodiment 2)

[0042] (1) Add 100g of water, 2g of allyloxy nonylphenol polyoxyethylene ether ammonium sulfate, 60g of styrene, 50g of butyl methacrylate, and 3g of acrylic acid into the emulsification container with stirring in order and turn it at 200r / min rotating speed to disperse at high speed to obtain pre-emulsion.

[0043](2), 150g of water, 2g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 80g of isooctyl acrylate, 150g of octadecyl methacrylate, 50g of hydroxypropyl methacrylate, 5g of acrylic acid, Add 2g of A-174 into the emulsification container with stirring in order and disperse at a high speed of 200r / min to obtain a pre-emulsion.

[0044] (3) Add 3g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 20g of silica sol, 1g of sodium bicarbonate and 250g of water into a stirred reaction vessel, stir at a low speed of 50r / min and Heat to 84°C and add an aqueous solution containing 0.5g sodium persulfate, and at the same time drop the pre-emulsion (1...

Embodiment 3)

[0049] (1) Add 120g of water, 2g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 50g of styrene, 80g of isobornyl methacrylate, and 2g of acrylic acid into the emulsification container with stirring in order and 200r / min high-speed dispersion to obtain pre-emulsion.

[0050] (2) Put 160g of water, 2g of allyloxynonylphenol polyoxyethylene ether ammonium sulfate, 120g of isooctyl acrylate, 120g of methyl methacrylate, 40g of hydroxypropyl acrylate, 3g of acrylic acid, and 3g of A-174 in order Add it into an emulsification container with stirring and disperse at a high speed of 200r / min to obtain a pre-emulsion.

[0051] (3) Add 2g of allyloxy nonylphenol polyoxyethylene ether ammonium sulfate, 1g of allyloxy hydroxypropyl sulfonate, 10g of silica sol, 1g of sodium bicarbonate and 250g of water into a stirring tank In the reaction vessel, stir at a low speed of 50r / min and heat it to 84°C, add an aqueous solution containing 0.5g sodium persulfate, and add the pre...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
hardnessaaaaaaaaaa
Login to view more

Abstract

The invention relates to a silica sol hybrid hydroxyl acrylate emulsion and a preparing method thereof. A semi-continuous seed emulsion polymerization method is adopted, a hard monomer serves as a core, hard and soft monomers and a hydroxyl acrylatemonomer serve as a housing, organic silane is added into the housing to conduct modification, emulsifiers are all reactive emulsifiers, a sulfonate-modified HDI curing agent (Aquolin-268) of Wanhua Company is selected, and the ratio of the reactive emulsifiers tothe sulfonate-modified HDI curing agent is 10:1. The hardness of film reaches 3H, the silica sol hybrid hydroxyl acrylate emulsion is high in gloss and adhesive force and excellent in water resistance and alcoholresistance, and all other physical and chemical propertiescan meet nationalstandard requirements.

Description

technical field [0001] The invention relates to a preparation method of an emulsion for water-based wood paint, and specifically provides a silica sol hybrid hydroxyacrylate emulsion and a preparation method thereof. Background technique [0002] Acrylate emulsion has the advantages of low cost, good weather resistance, high gloss, and water-based environmental protection. It is the fastest-growing environmental-friendly coating adhesive for water-based coatings. The waterborne two-component acrylate polyurethane coating is composed of a hydrophilic modified -NCO-containing low-viscosity polyisocyanate curing agent and -OH-containing waterborne polyacrylate polyol. The water-based hydroxyacrylic emulsion has adjustable polymer structure, designable emulsion particle configuration, and can also be endowed with various functional designs. Due to the diversity, adjustability and designability of hydroxyl resin, the two-component acrylate polyurethane coating has high performan...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C08F283/06C08F212/08C08F220/06C08F220/18C08F220/20C08F220/14C08F2/44C08K3/36C09D175/04C09D5/16
CPCC09D175/04C08F2/44C08F212/08C08F220/06C08F220/18C08F220/20C08F283/065C08K3/36C09D5/1662C08F220/1804C08F220/1806C08F220/1818C08F220/1808
Inventor 王海泉黄道明
Owner 江苏日出化工有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products