Method for preparation of lignite resin drilling fluid loss additive
A technology of fluid loss reducer and lignite resin, which is applied in the directions of drilling compositions, chemical instruments and methods, etc., can solve the problems of easy foaming, difficult to control reaction and condensation process, and no visibility.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0031] 1. Preparation of lignite resin fluid loss additive
[0032] (1) Add water 50g, lignite 26.5g, acrylic scrap 10.5g, polyether polyol 5.6g, sodium hydroxide 3.2g, potassium hydroxide 4.2g, sodium bisulfite 0.55g, sodium metabisulfite into the reactor in turn 0.55g, boric acid 0.25g, zirconium chloride 0.35g, formaldehyde 0.6g.
[0033] (2) Turn on the stirring device, stir the mixture in the reactor uniformly for 30 minutes, heat the reactor to a temperature of 130°C, react at a constant temperature for 4 hours, stop stirring and heating, and spray dry to obtain a solid powder product of the lignite resin filtrate reducer.
[0034] 2. Performance evaluation of lignite resin filtrate reducer
[0035] (1) Reduce fluid loss and rheology
PUM