Preparation method of ozone heterogeneous oxidation solid catalyst
A heterogeneous oxidation, solid catalyst technology, applied in catalyst activation/preparation, physical/chemical process catalyst, catalyst carrier, etc., can solve the problems of poor anti-toxicity, low catalyst adsorption, easy to lose catalytic activity, etc. Adsorptive, inhibiting precipitation, improving anti-toxicity and catalytic activity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0007] Embodiment 1:1.4g lithium hypochlorite, 1.7g two (acetylacetonate) beryllium, 140ml deionized water, join volume and be that in the sealable reactor of 500ml, stir and mix evenly, the weight concentration of this aqueous solution is 2.2%, times Lithium chlorate: the weight ratio of bis(acetylacetonate) beryllium=1:1.2; add deionized water to wash to neutral, dry at 103°C to remove moisture, and then sieve 2.8g erionite of -200 mesh to +400 mesh standard sieve , 3.8g garnet, 4.7g light shale ceramsite, 5.8g pyrophyllite, 6.7g expanded vermiculite, 7.8g calcium alumina feldspar, lithium hypochlorite and bis(acetylacetonate) beryllium weight (3.1g): Porous The weight of the material (31.6g) = 1:10.2, heat up to 36°C, continue to stir and react for 3.2h, filter, and dry at 103°C to obtain a pore-expanding modified carrier of 30g; in a 500ml ultrasonic reactor, put the pore-expanding modified Carrier 30g, add the aqueous solution that 3.3g dodecyltrimethylammonium chloride i...
Embodiment 2
[0008] Embodiment 2: 0.24g lithium hypochlorite, 0.36g bis(acetylacetonate) beryllium, 10ml deionized water, join volume and be that in the sealable reactor of 100ml, stir and mix evenly, the weight concentration of this aqueous solution is 5.7%, times Lithium chlorate: the weight ratio of bis(acetylacetonate) beryllium=1:1.5; add deionized water to wash to neutral, dry at 103°C to remove moisture, and then sieve 1.45g erionite of -200 mesh to +400 mesh standard sieve , 1.65g garnet, 1.85g light shale ceramsite, 2.05g pyrophyllite, 2.25g expanded vermiculite, 2.45g calcium alumina feldspar, lithium hypochlorite and bis(acetylacetonate) beryllium weight (0.6g): Porous The weight of the material (11.7g)=1:19.5, heat up to 48°C, continue to stir and react for 5.8h, filter, and dry at 105°C to obtain a pore-expanding modified carrier of 11.5g; put it into a 100ml ultrasonic reactor Modified carrier 11.5g, add the aqueous solution that 2.2g dodecyltrimethylammonium chloride is diss...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com