Anti-corrosion and antibacterial high-molecular polymeric furniture board and preparation process thereof
A polymer polymerization, anti-corrosion and anti-bacterial technology, applied in wood treatment, impregnated wood, manufacturing tools, etc., can solve the problems of lack of anti-bacterial and anti-fouling effects, lack of anti-bacterial ability, low anti-bacterial ability, etc., to achieve improved anti-bacterial and disinfection effects, excellent Antibacterial effect, effect of improving adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] An antiseptic and antibacterial polymer furniture board and a preparation process thereof, comprising the following steps:
[0021] 1) Dehydration treatment of the sheet substrate: place the sheet substrate inside the autoclave and dry it at a low pressure with a drying pressure of 0.25Mpa and a drying time of 5 hours. The drying temperature for the first 2 hours is 45°C and the remaining temperature is 200°C. ℃, then turn off the temperature, and release the pressure, and take out the dehydrated sheet substrate;
[0022] 2) Preparation of preservatives: the emulsifier, copper naphthenate, diatomaceous earth, lignin, calcium propionate, titanium diboride, sodium benzoate, acetic acid, tributyl phosphate, pyrithione and ethanol Mix and stir for 20 minutes;
[0023] 3) Preparation of wet gel: Mix and stir polysiloxane, water, solvent and catalyst in parts by weight for 1-3 hours, then add silver nanoparticles and titanium dioxide to the stirred raw materials, stir for 20...
Embodiment 2
[0032] An antiseptic and antibacterial polymer furniture board and a preparation process thereof, comprising the following steps:
[0033] 1) Dehydration treatment of the sheet substrate: place the sheet substrate inside the autoclave and dry it at low pressure, the drying pressure is 0.50Mpa, the drying time is 2 hours, the drying temperature is 45°C for the first 1 hour, and the remaining temperature is 230°C ℃, then turn off the temperature, and release the pressure, and take out the dehydrated sheet substrate;
[0034] 2) Preparation of preservatives: the emulsifier, copper naphthenate, diatomaceous earth, lignin, calcium propionate, titanium diboride, sodium benzoate, acetic acid, tributyl phosphate, pyrithione and ethanol Mix and stir for 30min;
[0035] 3) Preparation of wet gel: Mix and stir the polysiloxane, water, solvent and catalyst in parts by weight for 2 hours, then add silver nanoparticles and titanium dioxide to the stirred raw material, stir for 30 minutes, ...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com