Novel composite efficient VOCs comprehensive waste gas treatment catalyst and preparation method thereof
A waste gas treatment and composite technology, applied in the direction of catalyst activation/preparation, physical/chemical process catalysts, chemical instruments and methods, etc., can solve the problems of low conversion rate of VOCs, easy poisoning of catalysts, single catalytic activity, etc., and achieve recyclability Strong resistance, no secondary pollution, low conversion temperature
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0040] Preparation Example novel compound of formula VOCs efficiently integrated exhaust gas treating catalyst according to the present embodiment, comprising the steps of:
[0041]1) High-negative carrier system: The carrier is 30%, 40% silica, 13% magnesium oxide, 3% oxide, and calcium oxide, and 3% oxide. Diliborn nitric acid is added to the stirring tank, the mass of dilute nitric acid is controlled by 15% of the overall solid mass, and the dilute nitric acid pH is controlled at 4-6, and the stirring frequency of the stirring can is controlled at 30-60 rpm, and the stirring time is controlled From 1-2h, a uniform carrier feedstock is obtained, and the carrier feedstock is placed in a honeycomb mold forming apparatus for extrusion molding (100 * 100 * 50, unit mm) 200 mesh, and put the molded carrier into the drying oven for drying The drying temperature is controlled at 80 ° C to 130 ° C, and the drying time is controlled at 8-16 h. After drying, the dried carrier is placed in...
Embodiment 2
[0046] Example 2 1) High negative load bearer is made as in Example 1, and in different, the carrier is 50%, 20%, magnesium oxide, 3% oxide, 3% oxide, and calcium oxide, and calcium oxide, and calcium oxide by 3% oxide. The hydrocarbonite 8% is mixed, and the carrier feedstock is placed in a honeycomb mold forming apparatus for extrusion molding (100 * 100 * 100, unit mm) 400 mesh;
[0047] 2) The underlying anti-high temperature modification step is the same as in Example 1, and the total concentration of the metal ion concentration of the mixed solution is controlled at 5 mol / L, the coating amount is controlled at 8% of the weight of the carrier;
[0048] 3) The medium-level high dispersion modification step is the same as in Example 1, and the metal ion concentration of the mixed solution is controlled at 3 mol / L;
[0049] 4) Highly active substance mushroom steps as in Example 1, different, the metal ion concentration of the mixed solution is controlled at 7 mol / L;
[00...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com