Ozone heterogeneous oxidation solid catalyst preparation method
A heterogeneous oxidation, solid catalyst technology, applied in heterogeneous catalyst chemical elements, physical/chemical process catalysts, metal/metal oxide/metal hydroxide catalysts, etc. Toxic adverse effects, catalyst loss of catalytic activity, easy to lose catalytic activity and other problems, to achieve good environmental and economic benefits, enhance anti-toxicity, inhibit the effect of precipitation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0007] Embodiment 1:1.35g lithium hypochlorite, 1.65g bis(acetylacetonate) beryllium, 140ml deionized water, join volume and be that in the sealable reactor of 500ml, stir and mix evenly, the weight concentration of this aqueous solution is 2.1%, times Lithium chlorate: the weight ratio=1:1.2 of bis(acetylacetonate) beryllium; add 2.75g activated carbon, 3.75g carnallite, 4.75g potassium feldspar, 5.75 Weight of g boromagnesite, 6.75g illite, 7.75g coal gangue, lithium hypochlorite and bis(acetylacetonate) beryllium (3g): weight of porous mineral material (31.5g)=1:9.5, heat up to 36°C , continue to stir and react for 3.2h, wash and filter, and obtain 31g of pore-enlarging modified carrier after drying to constant weight; in a 500ml ultrasonic reactor, put 31g of pore-enlarging modified carrier, and then add 3.25g of methacryloxyethyl chloride Trimethyl ammonium chloride was dissolved in 100ml of deionized water in an aqueous solution, the weight concentration of the aqueous s...
Embodiment 2
[0008] Embodiment 2:0.24g lithium hypochlorite, 0.36g bis(acetylacetonate) beryllium, 10ml deionized water, join volume and be that in the sealable reactor of 100ml, stir and mix evenly, the weight concentration of this aqueous solution is 5.7%, times Lithium chlorate: the weight ratio=1:1.5 of bis(acetylacetonate) beryllium; add 1.45g activated carbon, 1.65g carnallite, 1.85g potassium feldspar, 2.05 The weight of g boromagnesite, 2.25g illite, 2.45g coal gangue, lithium hypochlorite and bis(acetylacetonate) beryllium (0.6g): the weight of porous mineral material (11.7g)=1:19.5, heated to 48 ℃, continue to stir and react for 5.8 hours, wash and filter, dry and constant weight to obtain 11.5g of pore-expanding modified carrier; put 11.5g of pore-expanding modified carrier into a 100ml ultrasonic reactor, and then add 2.2g of methacryloyl chloride An aqueous solution of oxyethyltrimethylammonium dissolved in 26ml of deionized water, the weight concentration of the aqueous solut...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com