Environment-friendly water-based paint coating and preparation method thereof
A water-based paint and coating technology, applied in anti-fouling/underwater coatings, anti-corrosion coatings, polyester coatings, etc., can solve problems such as environmental pollution and volatile odors of coatings, secondary pollution of air and sewage, etc. Achieve the effect of improving tissue strength and cohesion, improving use quality and excellent mechanical quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] The invention provides a technical solution: an environmentally friendly water-based paint coating, in parts by weight, its raw material composition includes: 53 parts of polyester resin emulsion, 27 parts of polyurethane emulsion, 12 parts of melamine resin, 8 parts of activated carbon, 2 parts of defoaming agent 1 part, 1 part of leveling agent, 7 parts of curing agent, 3 parts of thickener, 1 part of coupling agent, 1 part of pigment, 0.8 part of pH regulator and 37 parts of deionized water.
[0020] Further, the defoamer is water-based non-silicone fatty acid polymer, and the leveling agent is carboxymethyl cellulose.
[0021] Further, the curing agent is an isocyanate curing agent, and the thickener is hydroxyethyl cellulose.
[0022] Further, the coupling agent silane coupling agent KH-560, the pigment is a mixture of zinc powder, iron oxide red, and heavy stone powder in a weight ratio of 1:2:2, and the pH regulator is 2-amino-2-methyl- 1-propanol, adjust the pH...
Embodiment 2
[0028] The invention provides a technical solution: an environmentally friendly water-based paint coating, in parts by weight, its raw material composition includes: 55 parts of polyester resin emulsion, 25 parts of polyurethane emulsion, 15 parts of melamine resin, 6 parts of activated carbon, 3 parts of defoaming agent 2 parts, 2 parts of leveling agent, 10 parts of curing agent, 4 parts of thickener, 2 parts of coupling agent, 2 parts of pigment, 1 part of pH regulator and 40 parts of deionized water.
[0029] Further, the defoaming agent is a silicone compound, and the leveling agent is a polysiloxane-polyether copolymer.
[0030] Further, the curing agent is a mixture of low-molecular polyamide curing agent and m-phenylenediamine curing agent at a mass ratio of 10:1, which can be cured at room temperature, and can increase the toughness of the coating while appropriately improving heat resistance and thickening. The agent is polyurethane thickener.
[0031] Further, the ...
Embodiment 3
[0037] The invention provides a technical solution: an environmentally friendly water-based paint coating, in parts by weight, its raw material composition includes: 57 parts of polyester resin emulsion, 23 parts of polyurethane emulsion, 17 parts of melamine resin, 8 parts of activated carbon, 4 parts of defoaming agent 2 parts, 2 parts of leveling agent, 12 parts of curing agent, 6 parts of thickener, 3 parts of coupling agent, 2 parts of pigment, 1.5 parts of pH regulator and 43 parts of deionized water.
[0038] Further, the defoaming agent is polyether polysiloxane copolymer, and the leveling agent is carboxymethyl cellulose.
[0039] Further, the curing agent is a mixture of low-molecular polyamide curing agent and m-phenylenediamine curing agent in a mass ratio of 15:2, which can be cured at room temperature, and can increase the toughness of the coating while appropriately improving heat resistance and thickening. The agent is hydroxyethyl cellulose.
[0040] Further,...