The preparation method comprises the following steps that low-
cobalt martensitic steel stainless steel
powder and a binder are subjected to mixing and
granulation, feed is obtained, the feed is injected into a mold, an injection
green body is obtained,
solvent degreasing is conducted to obtain a dissolvable blank, warm isostatic pressing treatment is conducted to obtain a pressed
green body, and the pressed
green body is subjected to heat treatment to obtain the ultra-low-carbon low-
cobalt martensitic steel with the ultra-low-carbon low-
cobalt martensitic steel with the ultra-low-carbon low-cobalt martensitic steel. According to the preparation method, two times of
degreasing are adopted, after the injection blank is obtained through injection molding, a
solvent is adopted for
degreasing to remove part of the binder, and then the ultra-low-carbon and low-cobalt martensitic steel is obtained through
sintering in a vacuum environment, so that the ultra-low-carbon and low-cobalt martensitic steel is obtained. According to the ultra-low-carbon low-cobalt martensitic steel and the preparation method thereof, the low-carbon low-cobalt martensitic steel is subjected to temperature isostatic pressing treatment under the set technological parameter condition to obtain a green body, the inventor finds that the density of the green body can be greatly improved, and the ultra-low-carbon low-cobalt martensitic steel has
high density, fine grains and excellent mechanical properties.