The present application relates to the technical field of
cathode roller
titanium ring preparation, and discloses a preparation method of a welded and formed
cathode roller
titanium ring, comprising the following method steps: step one: opening a groove at both ends of a TA1
titanium plate
raw material, and butt jointing through a four-roll plate rolling
machine; step two: using
plasma automatic
welding to weld a longitudinal seam under high-purity
argon protection; step three: placing the welded and formed
titanium ring into an electric heat treatment furnace for high-temperature homogenization heat treatment; step four: using a ring rolling
machine to roll and deform the
titanium ring after heat treatment, with a deformation amount of greater than or equal to 40%; step five: correcting the shape of the
titanium ring after rolling, and performing overall recrystallization annealing heat treatment; and step six: after annealing, using a
numerical control vertical lathe to perform turning
processing on the inner wall of the titanium ring, and waiting for subsequent hot charging processes to be used. Compared with the
spinning forming process commonly used in China at present, the process flow of the present application is short, the production efficiency is high, the axial and radial directions of the semi-finished titanium ring are fixed through one driving source, the operation is simple, and the manufacturing cost is lower.