The invention discloses an efficient
separation method for treating high-
talc-content and high-
sulfur copper ore, which comprises the following steps: S1, potential regulation and control of raw ore pulp: directly adding a pH
regulator, an activating agent and a dispersing agent for ore
grinding to regulate the potential of the ore pulp, and
grinding the high-
talc-content and high-
sulfur copper ore until-0.074 mm accounts for 60-85% for later use; a mixed inhibitor and a
copper collecting agent are sequentially added to the ore pulp roughing subjected to ore pulp potential regulation and control in the step S1 for preferential copper flotation,
scavenging copper rough concentrate and
tailings are obtained through one-time roughing and two-time
scavenging, and middlings are sequentially returned; s3, copper rough concentrate concentration is conducted, specifically, a pH
regulator, a dispersing agent and a mixed inhibitor are sequentially added into the copper rough concentrate obtained through roughing in the S2 for two times of concentration, copper concentrate and first-concentration
tailings are obtained, and middlings are returned in sequence; the preparation method has the beneficial effects that an aluminum salt
polymer and a
macromolecule react in advance to form a special molecular structure which is adsorbed to the surface of
talc, so that the surface of the talc is subjected to hydrophilic modification, and the effect of efficiently inhibiting the talc is achieved.