The invention discloses a flat paint for furniture. The flat paint is composed of the following raw materials (by weight): 1.4-3 parts of 2,2,4-trimethyl-1,3-pentanediol monoisobutyrate, 0.7-2 parts of PTMEG, 0.8-2 parts of p-toluenesulfonamide, 10-12 parts of tung oil, 0.06-0.07 part of sodium hydroxide, 3-4 parts of methanol, 0.1-0.2 part of perfluorosulfonate resin, 6-8 parts of acetic acid, 10-15 parts of 26-30% hydrogen peroxide, 10-17 parts of tetraethyl orthosilicate, 0.1-0.2 part of Y-chloropropyltrimethoxysilane, 70-80 parts of unsaturated polyester resin, 0.6-1 part of methylethyl ketone peroxide, 15-20 parts of barite powder, 1-2 parts of naphthenic soap, 0.8-2.2 parts of lauryl alcohol phosphoric acid ester potassium, 1-2 parts of phenylimidazoline, 0.8-1 part of calcium alginate, 3-5 parts of titanium dioxide and 0.2-0.4 part of polyoxyethylene octylphenol ether. By adding titanium dioxide and barite powder into the paint, effective effects can be achieved, and decorative performance of a film is enhanced.