The invention discloses a preparation method of a high-performance soft
magnetic powder core, which comprises the following steps: S1, dissolving
nitrate in an
organic solvent, and uniformly stirring; s2, adding a
silane coupling agent, and uniformly stirring; s3, keeping the pH value in an alkaline range all the time; s4, deionized water is added into the solution obtained in the step S3, then soft
magnetic powder is added, stirring is continuously conducted after the temperature is adjusted, and
drying is conducted after the solution is completely evaporated; s5, carrying out preheating treatment under the protection of
inert gas to prepare nanoscale
oxide coated soft
magnetic powder; s6, adding organic
silicon resin into a
methyl acetate or
dimethyl carbonate solution, uniformly stirring, pouring into the coated soft magnetic
powder obtained in the step S5, stirring until the solution is completely volatilized,
drying, adding a
lubricant, and uniformly mixing and stirring; and S7, the
powder is subjected to heat treatment in the
nitrogen atmosphere after being subjected to
compression molding, and the high-performance soft magnetic
powder core is prepared. Compared with the prior art, high performance stability and low loss are both considered.