The invention provides an Nbc nanoparticle reinforced X80 plastic pipe steel plate and a production method of the Nbc nanoparticle reinforced X80 plastic pipe steel plate. The steel plate comprises, by weight percentage, 0.06%-0.12% of C, 0.10%-0.30% of Si, 0.60%-1.40% of Mn, 0.07%-0.15% of Nb, 0.001%-0.004% of N, 0.01%-0.04% of Ti, 0.025%-0.045% of Al, not larger than 0.010% of P, not larger than0.005% of S, not larger than 0.30% of Cu, not larger than 0.30% of Mo, 0.12%-0.30% of Cr, 0.12%-0.30% of Ni and the balance Fe and inevitable impurity elements. The production method comprises the steps of material preparation, converter or electric furnace smelting, secondary refining, casting, slab reheating, controlled rolling and controlled cooling. By the adoption of the produced steel plate, the safety of oil and gas transmission pipelines laid in geological complex areas is ensured, and the purposes of high-pressure transportation of natural gas and oil and the like are met.