The invention discloses a
copper-
tungsten alloy-
copper-steel composite electrical contact and a preparation method thereof, and relates to the technical field of
alloy material preparation. Comprising the following steps: performing
compression molding on
tungsten powder to obtain a blank block; pre-
sintering the
briquette to prepare a framework, so as to obtain a
tungsten framework; the theoretical
copper infiltration weight is calculated according to the weight of the tungsten framework, copper infiltration is conducted on the tungsten framework according to 1.2-1.4 times of the theoretical copper infiltration weight, and the copper-
tungsten alloy is obtained; the method comprises the following steps: respectively
machining and cleaning a copper-
tungsten alloy, a steel part and a copper part, then assembling, placing a
chromium-
copper alloy on the top of the assembled copper part, vacuumizing,
sintering at 1250-1300 DEG C, and cooling to obtain a blank; and carrying out heat treatment on the blank to obtain the copper-
tungsten alloy-copper-steel composite electrical contact. According to the method, the copper-tungsten
alloy, the copper and the steel are combined, the
bonding strength between matrixes is improved, the consistency and the stability of the quality of a welded product are guaranteed, and the air hole defect of a bonding surface is reduced.