The invention relates to the technical field of composite wall materials, in particular to a
flame-retardant and anti-aging composite
wall material and a preparation process thereof. The waterproof
coating comprises the following components: 0.5 to 1.5 parts by weight of an
antioxidant, 13 to 17 parts by weight of
Portland cement, 2 to 4 parts by weight of
epoxy resin, 1 to 3 parts by weight of
polyurethane, 0.8 to 1.2 parts by weight of an
ethylenediamine curing agent, 2 to 6 parts by weight of
glass fiber, 4 to 8 parts by weight of aluminum
hydroxide, 3 to 11 parts by weight of 2-
diphenylphosphine ethanethiol, 2 to 4 parts by weight of a
polydimethylsiloxane waterproof agent and 2-(2-
diphenylphosphine ethanethiol). The component A comprises the following components in parts by weight: 0.1-0.5 part of 2 '-hydroxy-5'-methylphenyl)
benzotriazole, 0.2-0.4 part of lauryl
sodium sulfate and 55-65 parts of a
fly ash filling material; wherein the
antioxidant is prepared by mixing
amifostine mercaptan and a
coupling agent according to a
molar ratio of 1: (1.0-1.2); the
coupling agent is prepared by mixing
hexamethylene diisocyanate and gamma-glycidyl propyl trimethoxy
silane; the curing agent is a mixture of a curing agent and a curing agent; the
antioxidant is adopted, so that the anti-aging and
flame-retardant effects of the
wall material are improved, the interface compatibility is improved, and the stability of the material is improved.