The invention discloses a
processing method of a rolled abutting-against leather type kitten
heel outer sole for men. The method includes the steps that the thickness of the half sole part is selected to be 3.5 mm or more, the part of the outer sole,10mm-15mm back from the metatarsal-phalangeal line towards the heelpiece part, is gradually
cut thinner until the thickness at the
heel breast reaches 1mm to 1.5mm; the length of rolled leather which adheres to the
heel breast is 0.5 mm-0.8 mm larger than the height of the heel breast; coarse grain
abrasive cloth or a
tin fillet is used for sanding; a welt needs to be soaked in water for one minute and then stands for half an hour after being taken out so that the
moisture content of the welt can reach 18-24%, the edge of the outer sole abuts against a backer of a milling
machine, and the inner side edge of the welt is close to a
milling cutter, so that the redundant inner side of the welt is removed through milling; after the edge is milled, sanding treatment is performed, it is only required that the outer sole surface is upturned to be placed on a backing plate, a heated
trademark male die is pressed into the outer sole surface, and then heat shaping is performed for several seconds. According to the method, the production process of the kitten heel outer sole for men can be strictly controlled, so that the
production quality of the outer sole meets requirements, the service life of the outer sole is guaranteed, and the outer sole is comfortable and safe to wear for people.