The invention relates to a method for producing molten iron by adding 
scrap steel into a 
blast furnace. The method mainly comprises the steps of mixing, distributing, 
smelting, iron runner modification, iron runner distribution, molten iron 
ladle distribution, molten iron 
ladle baking and tapping and the like. According to the method, the 
scrap steel is added in different 
modes in different opportunities in a 
blast furnace smelting process, so that the technical effects that the overall 
smelting time is shortened, the tapping amount is improved, the utilization amount of the 
coke is greatly saved, and the downstream degree of the 
blast furnace and the like are improved. According to the method, the 
utilization rate of scarp steel can be greatly improved, more industry and domestic scarp steel can be digested, 
energy consumption can be reduced, emission of harmful substances is reduced, the development requirements of 
environmental protection and 
energy conservation are met, and important 
social benefits are achieved while the blast furnace 
economic benefits are increased.