The invention discloses a
basalt fiber preparation method, a mineral mixture and a production technology. The preparation method comprises the step of
grinding the mineral mixture into 200 to 300-meshpowder to obtain
basalt fibers. The mineral mixture is prepared from the ingredients in weight percentage: 47% to 59% of SiO2, 11% to 16% of Al2O3, 5% to 9% of CaO, 2% to 7% of MgO, 2% to 5% of Na2O,0.5 to 3% of K2O, 0 to 2.6% of Li2O, 7% to 16% of Fe2O3, 1% to 3.4% of TiO2, 0 to 3% of ZrO2, 0 to 2% of CeO2 and 0 to 2% of MnO. The used mineral mixture is prepared from varieties of ores, so thatthe whole ingredient fluctuation range is reduced to the lowest, wiredrawing performance is improved, mineral mixture ingredient contents and mutual proportional relation are controlled, strength is improved, stability is improved, elasticity modulus is improved, a
melting temperature is reduced, energy is saved,
glass material characteristics are changed, and improving wiredrawing performance isachieved.