The invention relates to the technical field of
continuous casting, in particular to a control method of transverse corner cracks of a
casting blank of a chamfering crystallizer. The control method includes the steps that the spraying angle of spray nozzles on a first foot roll, a second foot roll, a third foot roll and a fourth foot roll relative to the
casting blank is controlled to range from 95 degrees to 110 degrees; and the
water flow of primary cooling water of the
narrow face of the chamfering crystallizer is controlled to range from 520 L / min to 600 L / min. According to the control method of the transverse corner cracks of the
casting blank of the chamfering crystallizer, the spraying angles of the spray nozzles on the first foot roll, the second foot roll, the third foot roll and the fourth foot roll relative to the casting blank are controlled to range from 95 degrees to 110 degrees, the
cooling effect of the chamfering portion of the casting blank of the chamfering crystallizer for
microalloyed steel can be fully guaranteed, and meanwhile the influence on the following process of the casting blank is avoided; and in addition, the
water flow of the primary cooling water of the
narrow face of the chamfering crystallizer is controlled to range from 520 L / min to 600 L / min, and the transverse corner cracks can be prevented from being generated on the casting blank of the chamfering crystallizer for the
microalloyed steel.