The invention discloses a modified resin composition, which includes the following components of, by weight, 35% to 95% of 
polyamide, 4% to 15% 
laser sensitive additives and 1% to 60% of other additives, and the added weight of the total content is 100%. The chemical general formula of the 
laser sensitive additives is XY2O4, and the 
laser sensitive additives are of isometric 
crystal system with the 
axial length a=b=c and the axial 
angle alpha=beta=gamma=90 degrees; a tetrahedral atom is a 
metal atom from an IIIA group, an IB group, an IIB group, a VIB group, a VIIB group and a VIII group of 
periodic table of the elements, wherein the 
metal atom includes one of 
chromium, 
manganese, iron, 
cobalt, 
nickel, 
copper, 
zinc, 
palladium and aluminum, preferably one of 
transition metal chromium, 
manganese, 
copper and 
metal palladium; and an octahedral atom is a metal atom from an IIIA group, an IB group, an IIB group, a VIB group, a VIIB group and a VIII group of 
periodic table of the elements, wherein the metal atom includes one of 
chromium, 
manganese, iron, 
cobalt, 
nickel, 
copper, 
zinc, 
palladium and aluminum, preferably one of 
transition metal chromium, manganese, copper and metal palladium. The modified resin composition has the advantages of being high in 
processing temperature and small in space among metal wires.