The invention relates to a preparation method of a neodymium-iron-boron magnet with an adjustable grain boundary. The performance of the neodymium-iron-boron magnet is controlled through regulation ofthe grain boundary, a diffusion source and the neodymium-iron-boron magnet form a neodymium-iron-boron magnet intermediate, the chemical components of the neodymium-iron-boron magnet intermediate areexpressed, in percentage by mass, as [R1xR2yR3<1-x-y>]aMbBcFe<100-a-b>, wherein x is greater than or equal to 0.8 and less than or equal to 1, y is greater than or equal to 0 and less than or equal to 0.08, a is greater than or equal to 32 and less than or equal to 38, b is greater than or equal to 0.5 and less than or equal to 7, c is greater than or equal to 0.9 and less than or equal to 1.2, R1 refers to one or more of Nd, Pr and Ce, R2 refers to one or more of La and Sm, R3 refers to one or more of Tb, Dy and Ho, M refers to multiple groups of Al, Cu, Ga, Ti, Co, Mg, Zn, Nb, Mo and Sn, and then the neodymium-iron-boron magnet intermediate is charged into a furnace and subjected to high-temperature aging treatment. The coercive force performance of the heavy-rare-earth-free magnet canbe higher than 25 kOe, and the coercive force performance of the heavy-rare-earth-containing magnet after treatment can be higher than 29 kOe.