The invention discloses green low-carbon high-rutting-resistance
asphalt concrete and a preparation method thereof, and relates to the technical field of
asphalt concrete. The technical scheme is as follows: RAP accounts for 30-40% of the
mass of a new aggregate, 53-65 parts of the new aggregate, 3.2-4.1 parts of new
asphalt, 4-6 parts of mineral
powder, 0.3-0.4 part of high-density oxidized
polyolefin, 0.05-0.1 part of a
drying agent, 0.05-0.1 part of a
lead salt stabilizer, 0.05-0.1 part of an auxiliary agent, 1.5-3 parts of reactive
polyurethane, 3-6 parts of a
polyester modifier, 0.5-2 parts of a
silane coupling agent, 0.1-0.5 part of an
antioxidant and 0.5-2 parts of a dispersing agent. Through the synergistic effect of high-density oxidized
polyolefin and reactive
polyurethane, the performance of aged asphalt in RAP is improved, the rutting resistance of
asphalt concrete is improved, VOC emission is reduced, the
sustainability of the material is enhanced, the long-term durability is improved, and the service life of a road is prolonged.