The invention discloses a preparation method of a carbon fiber whisker contact net lead, and the contact net lead comprises a carbon fiber, a whisker, metal conducting media and additives. The carboncontent of the carbon fiber is not less than 90 percent, and the tensile strength is not less than 3500MP; the whisker is a zinc oxide whisker, a calcium sulphate whisker, a magnesium sulphate whisker, a magnesia whisker or a silicon carbide whisker; the metal conducting media are copper, silver, aluminum, magnesium and zinc or a copper alloy, a silver alloy, an aluminum alloy, a magnesium alloy and a zinc alloy; and the additives are nickel, tin and niobium. The integral contact net lead is in an annular structure, and two V-shaped notches are laterally symmetrically arranged at the upper part of one half of an outer ring. The carbon fiber whisker contact net lead has the characteristics of high tensile strength, large elastic modulus, good flexibility, light weight and easy installation,has the key characteristics of small change of lead tension and sag along with air temperature, and is suitable for the requirement of the power supply engineering of high speed railway contact netsor urban track traffic contact nets.