The invention discloses a novel sensitive coating prepared from, by weight, 30-50 parts of organic silicon modified epoxy acrylic acid, 0.2 parts of cobalt oxide crystal, 2 parts of water, 3-5 parts of nano cellulose filament, 60 parts of bismuth vanadate, 20-30 parts of polyvinyl alcohol, 18 parts of aluminum oxide, 12 parts of sepiolite powder, 20-30 parts of talcum powder, 20 parts of mica powder, 6-10 parts of organic silicon coupling agent, 20-30 parts of xylene, 2-4 parts of a dispersant, 1-3 parts of an anti-settling agent, 3-5 parts of a defoamer, and 0.2 parts of Bi2WO6.