The invention provides a glass fiber reinforcement PP material with low VOC and a preparation method of the glass fiber reinforcement PP material. A pp material is adopted as a base material, by adding extracting agent master batch, on the premise of not changing equipment, VOC is removed from the interior of the material rather than being absorbed by a porous material or remaining in the material by virtue of the blocking of a deodorizing agent, and the method has good effect for reducing the VOC; moreover, the complexity of the processing technology is not increased; less extracting agent master batch is used, and by adding 1.5 to 3.5 parts by weight of extracting agent master batch, the requirement of people on PV3900 and PV3341 can be met; by adding a grafting agent, an antioxidant and glass fibers, mechanical properties of the PP material are improved, the tensile strength is 94MPa or higher, the elongation at break is 3.1 percent or higher, the bending modulus is 7800MPa or higher, a melt index is 3.4 g/10min or higher, and the impact strength is 10.5KJ/m<2> or higher.