The application discloses a composite tailor-
welding method for improving the yield of an aluminum-
silicon coated plate integrated door ring, and belongs to the technical field of tailor-
welding methods.The method comprises the following steps: preparing a plurality of door ring blanking pieces, all of which are aluminum-
silicon coated plate materials; and connecting the blanking pieces into an integrated door ring by tailor-
welding, wherein the connection mode between one blanking piece and the adjacent two sides is
lap joint, the
lap joint strength at the two places is realized by resistance
spot welding, the other connections are butt joints, and the strength is realized by
laser tailor-welding, the
laser tailor-welding adopts a micro-sphere reinforced welding wire, and the preparation method of one of raw materials of the micro-sphere reinforced welding wire, porous micro-sphere composite
metal powder, is modifying
camphor by using cation
starch modified kaolin and
sodium lignosulfonate, and mixing the
camphor with Al-Si-Sr
alloy micro-sphere
powder to form pores.Through the above method, the yield of the aluminum-
silicon coated plate integrated door ring is improved.