The invention discloses a process method for preparing an
erosion type
tungsten-
rhenium thermocouple. The method comprises the following steps of:
polishing a
tungsten sheet and a
tungsten-
rhenium alloy sheet by using an electric grinder, removing stains on the surfaces of the tungsten sheet and the tungsten-
rhenium alloy sheet so that the tungsten sheet and the tungsten-rhenium
alloy sheet are smooth, and
welding a tungsten wire and the tungsten sheet as well as a tungsten-rhenium alloy wire and the tungsten-rhenium alloy sheet together through
electric resistance welding to form positive and negative electrodes of the
erosion type tungsten-rhenium
thermocouple; sequentially arranging an aluminum
oxide sheet, a tungsten sheet, an aluminum
oxide sheet, a tungsten-rhenium alloy sheet and an aluminum
oxide sheet to form a five-layer sensitive core body structure, applying pressure to the five-layer sensitive core body structure through a clamp, and putting the five-layer sensitive core body structure into a tubular furnace for hot pressed
sintering to form a sensitive core body block; smearing high-temperature glue on the aluminum oxide sheets on the two sides of the sensitive core block, stuffing into the stainless
steel tube shell, and curing the high-temperature glue by using a hot air gun, so that the sensitive core block is tightly connected with the stainless
steel tube shell.
Temperature measurement nodes are refreshed in a
grinding mode, long-term and repeated use of the tungsten-rhenium
thermocouple in an
erosion environment and a high-temperature aerobic environment is achieved, and meanwhile the preparation efficiency is effectively improved.