The invention relates to the technical field of plastic processing, in particular to a processing technology for degradable plastics, which is prepared by the following method: (1) adding nano-FeSO 4 solution and Na 2 CO 3 solution and nano-Si 3 N 4 Mix, ultrasonically disperse at 400-500Hz for 20-30min, dry at 40-50°C, grind into powder, then place in a muffle furnace at 400-500°C, under N 2 sintering, followed by adding chitosan, CaCO 3 , EPDM copolymer, poly-β-hydroxybutyrate and bifenthrin are mixed and ground into powder, then sodium tripolyphosphate solution and guanidine hydrochloride solution are added, stirred evenly, and dried to obtain a mixed powder; ( 2) Mix epoxy resin, glycerin, polylactic acid and the mixed powder in step (1), extrude with a twin-screw extruder, and then enter into an injection molding machine for molding. The invention prepares degradable plastics which are not easy to mildew, age and be bitten by insects.