The invention relates to the technical field of furnace
slag waste reutilization, and discloses a method for preparing harmless regenerated aggregate with excellent building performance by utilizing furnace
slag, and the method specifically comprises the following steps: S101, obtaining to-be-treated furnace
slag, crushing the furnace slag to obtain furnace slag aggregate with the particle size of 100-500 microns, and performing harmless treatment on the furnace slag aggregate; s102, weighing 120-200 parts by weight of slag aggregate and 50-60 parts by weight of matrix
asphalt, respectively adding the slag aggregate and the matrix
asphalt into the modifier, heating the slag aggregate and the matrix
asphalt, and continuously mechanically stirring the slag aggregate and the matrix asphalt for 30-50 minutes at the
heating temperature of 80-100 DEG C to obtain initial bonding aggregate; s103, an air blowing pump is additionally arranged on one side of the stirring tank where the aggregate is initially bonded, and a large amount of external air is discharged into the stirring tank. Through the formation of
hydrogen bonds, the binding power of the mixture of the matrix asphalt and the slag aggregate is increased by 2.2-2.5 times, and the molecular
mass of the macromolecular substance is large, so that the substance generates more
hydrogen bonds in the structure, and the binding power among the regenerated aggregates is improved.