The invention relates to a 
machining technology for a 
metal ceramic flange. The 
machining technology is characterized by comprising the steps that firstly, powdery raw materials are added into a container according to the weight ratio and are evenly stirred, and then a proper amount of water is added for even stirring; secondly, the surface of the inner wall of a die is coated with a layer of 
release agent, the die is filled with the raw materials, and the raw materials in the die are pressed through a pressing plate; thirdly, the die is heated to evaporate water in the 
flange, and then the 
flange in the die is pressed after 
evaporation; fourthly, die releasing is conducted on the formed flange, and then some burrs are 
cut; fifthly, the flange obtained after die releasing is put into a 
combustion furnace to be heated for 15 min to 25 min at the temperature 
ranging from 600 DEG C to 800 DEG C, and then 
sintering is conducted for 10 min to 20 min at the temperature 
ranging from 1200 DEG C to 1300 DEG C; sixthly, after 
sintering forming is conducted, the temperature is gradually reduced to 200 DEG C, and the flange is taken out and cooled to the 
room temperature; and seventhly, the cooled flange is checked, and some burrs are ground. According to the 
machining technology, the steps are simple, operation is easy, the produced flange is high in 
hardness and small in weight, and the production cost is saved.