The invention discloses a waterproof energy-saving heat insulation material, which is prepared from the following ingredients in parts by weight: 18 to 28 parts of
calcium silicate, 5 to 10 parts of diatomite, 30 to 50 parts of
sepiolite, 18 to 26 parts of waste
ceramic powder, 10 to 16 parts of pure acrylic ester, 20 to 30 parts of
open hole expanded
perlite, 3 to 8 parts of
antimony-based nanometer composite environment-friendly fire retardants, 8 to 14 parts of
magnesium sulfate, 4 to 9 parts of
polypropylene fiber, 2 to 5 parts of acrylic
emulsion, 6 to 12 parts of hydroxypropyl
methyl cellulose water-retaining agents, 5 to 14 parts of
stearic acid, 2 to 5 parts of aminopropyltriethoxysilane, 1 to 5 parts of
aldehyde acetone polycondensate, 8 to 14 parts of seaweed glue, 1 to 3 parts of 2-
acrylamide-2-methylpropane
sulfonic acid copolymers, 3 to 8 parts of dodecayl dimethyl
amine oxide and 5 to 12 parts of modified light
calcium carbonate. The waterproof energy-saving heat insulation material has the advantages that the heat insulation performance is good; the hydrophobic function is good; the material per se has good ventilation performance; the waterproof performance of the
thermal isolation and heat insulation material is good; the
room temperature favorably keeps stable; the waterproof energy-saving heat insulation material is used for improving the living comfort, prolonging the building service life, and reducing the heating heat loss and
cold air loss, so that the goal of reducing the
energy consumption is reached.