The invention discloses a production and preparation method for a
ceramic steel medical door. The production and preparation method comprises the following steps of C1,
cutting a steel plate into a door sheet with proper dimension according to the installation dimension; S2, preparing an anti-
rust coating, specifically, weighing raw materials, and mixing the raw materials under the action of ultrasonic
waves so as to obtain the anti-
rust coating; S3, preparing an anti-
radiation thin film, specifically, weighing raw materials, treating
powder under a
molten state through a
tape casting method through an extruding
machine so as to obtain the thin film, and carrying out double-roller
air drying, traction and reeling on the thin film so as to obtain the anti-
radiation thin film; and S4,
coating the outer end of the door sheet with a layer of paint, attaching the anti-
radiation thin film to the outer layer of the door sheet so as to obtain the
ceramic steel medical door. The method has theadvantages that the outer side of a steel door is coated with the anti-
rust coating, so that the medical door has the anti-rust characteristic, in addition, the appearance color of the steel door is strong in adjustability, the steel door is more attractive in appearance, uniform mixing is carried out by adopting an ultrasonic method, and the uniform
mixing effect is better.