This invention belongs to the field of micro-
coating protection and discloses an
organosilicon aerosol coating for
waterproofing precision instruments and its preparation method. The
organosilicon aerosol coating comprises, by weight, 4-6 parts of fluorinated
organosilicon, 2-3 parts of organosilicon-
acrylate resin, 30-40 parts of a first
solvent, 20-30 parts of a second
solvent, 1-1.5 parts of a
release agent, 0.5-1 parts of a leveling agent, and a certain amount of
propellant. This invention uses a first
solvent and a second solvent with different volatility properties to improve the self-leveling and film-forming quality of the microfilm after spraying, reducing surface micropore defects caused by excessive
evaporation and forming a good waterproof layer. Through the synergistic effect of fluorinated organosilicon and organosilicon-
acrylate resin as film-forming materials, the waterproof coating formed with the
release agent and leveling agent possesses both long-lasting
waterproofing and peelability. When used for the protection of precision instruments, the coating can be peeled off after a certain protection period without leaving residual
pollution on the instrument surface.