The invention relates to a manufacturing method of a 
fastener, in particular to a manufacturing method of a screw, and belongs to the 
machining field of 
alloy materials. The manufacturing method of the screw comprises the steps that a screw blank is obtained by sequentially conducting normalizing treatment, 
machining and heat treatment on steel; the heat treatment involves 
carburizing treatment and 
tempering treatment, and during 
carburizing treatment, the temperature is firstly increased to 890-910 DEG C, preserved for 70-90 min, then decreased to 880-900 DEG C, preserved for 30-50 min, decreased to 820-840 DEG C, preserved for 20-40 min, and finally decreased to the 
room temperature through 
air cooling; the 
tempering treatment temperature is 150-180 DEG C, and the 
tempering treatment time is 100-140 min; and the finished screw can be obtained by sequentially conducting oil and 
rust removal, activating treatment, blackening and passivating treatment on the screw blank. After 
carburizing treatment is conducted on the screw 
alloy steel, the screw is provided with a hard and abrasion-resistant surface and a tough core and has high low-temperature 
impact toughness and good 
machinability; through surface blackening, the 
mechanical property of the screw is further improved, the Rockwell 
hardness (HRC) of the screw reaches 58-63, the layer depth of the screw is 0.7-1.0, and the service life of the screw is greatly prolonged.