The invention discloses a corrosion-resistant and wear-resistant high strength electrophoretic aluminum profile and a preparation process thereof and belongs to the field of aluminum profile preparation. The corrosion-resistant and wear-resistant high strength electrophoretic aluminum profile is prepared from the following raw materials in percent by weight: 0.8-1.2% of Mg, 0.4-0.6% of Si, 0.2-0.4% of Ti, 0.22-0.3% of Fe, 0.06-0.1% of Cu, 0.08-0.12% of Zn, 0.06-0.08% of Cr, 0.12-0.18% of Mo and the balance of Al and inevitable impurities. The preparation process is simple and effective and convenient and rapid in process operation. By controlling the contents of Mg, Si, Fe, Cu and Zn reasonably, strengthening phases such as Al2Cu, Al2CuMg, Mg2Si, MgZn2 and the like are formed in the electrophoretic aluminum profile to strengthen the synergistic effect, refine crystals and improve grain distribution, so that performance, such as wear resistance and corrosion resistance, of the electrophoretic aluminum profile is improved. By matching Si, Ti, Fe, Cr and Mo, the grains are refined, the cast structure and the weld joint structure are refined, the recrystallization temperature is increased, the thermal stability of a material is improved, the intergranular corrosion is avoided, and the corrosion performance of the electrophoretic aluminum profile is improved.